Table 3: EPR peak current densities and degree of sensitization (DOS) for MA304LZ and SUS304L under three conditions, AR: As received condition, SEN: Sensitized at 600 ℃ for 24 hr, AN-SEN: Annealed at 1000 ℃ and sensitized at 600 ℃ for 24 hr.
MA304LZ | SUS304L | |||||
AR | SEN | AN-SEN | AR | SEN | AN-SEN | |
ia (A/m2) | 1000 | 949 | 1770 | 673 | 951 | 1450 |
ir (A/m2) | - | 63 | 473 | - | 53.3 | 120 |
DOS | 0% | 6.6% | 26.7% | 0% | 5.6% | 8.3% |