Table 2: Crystal structure parameters of Sm-doped CuO thin film.

2θ (deg)

hkl

d

a

b

c

b (deg)

D (nm)

 

 

(nm)

   

32.4

110

0.2761

0.46698

0.34543

0.52815

79.7

3.447

35.1

11-Jan

0.2554

2.786

38.5

111

0.2336

2.823

47.9

20-Feb

0.1897

3.243