Table 2: APS process parameters for the deposition of bond coat CoNiCrAlY coatings.

Sample

Gun

Ø Nozzle [mm]

Spray distance [mm]

Flowrate Argon [l/min]

Florate Hydrogen [l/min]

Current Intensity [A]

Chromium Oxide top-coat

F4

6

140

91

90

630

CoNiCrAlY bond-coat

F4

6

130

55

9

600